SpoolSpec

Filament drying catalog

Pick a dryer. See which spools can run the listed cycle.

Brand temps disagree. Oven, heatbed, and AMS — only where the manufacturer published them.

Bookmark this page after you pick a dryer — the choice stays in the URL. No substitute temps invented here.

48 products

Shop
Polymaker PolyLite PETGPETG65°C / 6h————Buy
Polymaker PETG (new formula)PETG60°C / 6h————Buy
Bambu Lab PLA BasicPLA50°C / 8h60–70°C / 12h45°C / 12h——Buy
Bambu Lab PETG BasicPETG65°C / 8h80°C / 12h65°C / 8h——Buy
Bambu Lab PLA-CF / GFPLA-CF50–60°C / 8h65–75°C / 12h45°C / 12hYes—Buy
Overture PLAPLA50°C / 7h————Buy
Overture PETGPETG65°C / 7h————Buy
Overture TPU 95ATPU70°C / 7h————Buy
Overture ABSABS75°C / 7h————Buy
Overture ASAASA75°C / 7h————Buy
Overture Easy PA (Nylon)PA95°C / 7h————Buy
Prusament PLA / rPLAPLA45°C / 6h————Buy
Prusament PETGPETG55°C / 6h————Buy
Prusament TPUTPU60°C / 5h————Buy
Prusament ASAASA80°C / 4h————Buy
Prusament PC BlendPC85°C / 5h————Buy
Prusament PC Blend Carbon FiberPC-CF90°C / 4h——Yes—Buy
Prusament PA11 Carbon FiberPA-CF90°C / 6h——Yes—Buy
Prusament PVBPVB45°C / 8h————Buy
Prusament WoodfillPLA45°C / 6h——Yes—Buy
Bambu Lab PLA MattePLA50°C / 8h60–70°C / 12h45°C / 12h——Buy
Bambu Lab PLA SilkPLA55°C / 8h65–75°C / 12h45°C / 12h——Buy
Bambu Lab PLA WoodPLA55–65°C / 8h70–75°C / 12h45°C / 12hYes—Buy
Bambu Lab ABSABS75–85°C / 8h90–100°C / 12hNot compatible——Buy
Bambu Lab ASAASA75–85°C / 8h90–100°C / 12hNot compatible——Buy
Bambu Lab TPU for AMSTPU70°C / 8h80–90°C / 12h65°C / 12h——Buy
Bambu Lab PCPC75–85°C / 8h90–100°C / 12hNot compatible——Buy
Bambu Lab PA6-CFPA-CF75–85°C / 8–12h90–100°C / 12hNot compatibleYes—Buy
Bambu Lab PETG-CFPETG-CF60–65°C / 8h75–85°C / 12h65°C / 12hYes—Buy
Polymaker PolyLite PLAPLA55°C / 6h————Buy
Polymaker PolyLite ABSABS70°C / 6h————Buy
Polymaker ASAASA70°C / 7h————Buy
Polymaker PolyFlex TPU95TPU70°C / 8h————Buy
Polymaker PolyLite PCPC75°C / 6h————Buy
SUNLU PLA / PLA+PLA50–55°C / 6–8h————Buy
SUNLU PETGPETG60–65°C / 6–8h————Buy
SUNLU ABSABS75–85°C / 6–8h————Buy
SUNLU ASAASA80°C / 6–8h————Buy
SUNLU TPUTPU50–60°C / 6–8h————Buy
SUNLU PLA-CFPLA-CF50°C / 6–8h——Yes—Buy
eSUN PLA+PLA50°C / 8h————Buy
eSUN PETG+PETG60°C / 8h————Buy
eSUN ABS+ABS60°C / 8h————Buy
eSUN eTPU-95ATPU55°C / 4h————Buy
ELEGOO Rapid PLA+PLA45–55°C / 8h————Buy
ELEGOO Rapid PETGPETG55–65°C / 8h————Buy
ELEGOO TPUTPU65–75°C / 6–10h————Buy
ELEGOO ABSABS65–75°C / 4–6h————Buy

Why brand rows matter

Overture PETG dries at 65°C / 7h. Prusament PETG lists 55°C / 6h. Polymaker PolyLite PETG lists 65°C / 6h. A generic “PETG = 60–65” answer is wrong for at least one of those spools.